งานวิจัย (Publications)
รายละเอียดงานวิจัย
Publication Details
Publication Name Surface Analysis Of Hydrophobicity of Thai Silk Treated by SF6 Plasma
First Author Asst. Prof. Dr.Pradoong Suanpoot,
Author Prof. Dr.Dheerawan Boonyawan, K. Kueseng, S. Ortmann, R. Kaufmann, C. Umongno, P. Nimmanpipug, T. Vilaithong
Corresponding Author Asst. Prof. Dr.Pradoong Suanpoot,
Year2008